Rana Roy Chaudhury wrote:
I made some progress with the glues. ..... Experimented using the scrap wood from the kit ..
I made copies of the plan and laminated the original.
The kit wood sands clean and smooth. However, even with the smoothest sandpaper, the scratch wood has real fine hairs sticking out. Is this good or bad? Will this get sorted out after I put the white glue / water primer coat on?
The scratch wood is a lot softer and pliable......I think the water content is higher. Is this OK? Should I dry it out? Leave it out to bake in the sun for a while? Will it shrink?
Huge frowns when I think about covering, but that's for later posts.
Apologies for such long posts and hope I am not violating forum protocol. Please do not hesitate to tell me if I am.
[/quote]Regards, Rana